The lifetime of a battery is affected by various aging processes happening at the electrode scale and causing capacity and power fade over time. Two of the most critical mechanisms are the deposition of metallic lithium (plating) and the loss of lithium inventory to the solid electrolyte interphase (SEI). These side reactions compete with reversible lithium intercalation at the graphite anode. Here we present a comprehensive physicochemical pseudo-3D aging model for a lithium-ion battery cell, which includes electrochemical reactions for SEI formation on graphite anode, lithium plating, and SEI formation on plated lithium. The thermodynamics of the aging reactions are modeled depending on temperature and ion concentration, and the reactions kinetics are described with an Arrhenius-type rate law. The model includes also the positive feedback of plating on SEI growth, with the presence of plated lithium leading to a higher SEI formation rate compared to the values obtained in its absence at the same operating conditions. The model is thus able to describe cell aging over a wide range of temperatures and C-rates. In particular, it allows to quantify capacity loss due to cycling (here in % per year) as function of operating conditions. This allows the visualization of aging colormaps as function of both temperature and C-rate and the identification of critical operation conditions, a fundamental step for a comprehensive understanding of batteries performance and behavior. For example, the model predicts that at the harshest conditions (< –5 °C, > 3 C), aging is reduced compared to most critical conditions (around 0–5 °C) because the cell cannot be fully charged.
This article presents the development, parameterization, and experimental validation of a pseudo-three-dimensional (P3D) multiphysics aging model of a 500 mAh high-energy lithium-ion pouch cell with graphite negative electrode and lithium nickel manganese cobalt oxide (NMC) positive electrode. This model includes electrochemical reactions for solid electrolyte interphase (SEI) formation at the graphite negative electrode, lithium plating, and SEI formation on plated lithium. The thermodynamics of the aging reactions are modeled depending on temperature and ion concentration and the reactions kinetics are described with an Arrhenius-type rate law. Good agreement of model predictions with galvanostatic charge/discharge measurements and electrochemical impedance spectroscopy is observed over a wide range of operating conditions. The model allows to quantify capacity loss due to cycling near beginning-of-life as function of operating conditions and the visualization of aging colormaps as function of both temperature and C-rate (0.05 to 2 C charge and discharge, −20 °C to 60 °C). The model predictions are also qualitatively verified through voltage relaxation, cell expansion and cell cycling measurements. Based on this full model, six different aging indicators for determination of the limits of fast charging are derived from post-processing simulations of a reduced, pseudo-two-dimensional isothermal model without aging mechanisms. The most successful aging indicator, compared to results from the full model, is based on combined lithium plating and SEI kinetics calculated from battery states available in the reduced model. This methodology is applicable to standard pseudo-two-dimensional models available today both commercially and as open source.
The measurement of the active material volume fraction in composite electrodes of lithium-ion battery cells is difficult due to the small (sub-micrometer) and irregular structure and multi-component composition of the electrodes, particularly in the case of blend electrodes. State-of-the-art experimental methods such as focused ion beam/scanning electron microscopy (FIB/SEM) and subsequent image analysis require expensive equipment and significant expertise. We present here a simple method for identifying active material volume fractions in single-material and blend electrodes, based on the comparison of experimental equilibrium cell voltage curve (open-circuit voltage as function of charge throughput) with active material half-cell potential curves (half-cell potential as function of lithium stoichiometry). The method requires only (i) low-current cycling data of full cells, (ii) cell opening for measurement of electrode thickness and active electrode area, and (iii) literature half-cell potentials of the active materials. Mathematical optimization is used to identify volume fractions and lithium stoichiometry ranges in which the active materials are cycled. The method is particularly useful for model parameterization of either physicochemical (e.g., pseudo-two-dimensional) models or equivalent circuit models, as it yields a self-consistent set of stoichiometric and structural parameters. The method is demonstrated using a commercial LCO–NCA/graphite pouch cell with blend cathode, but can also be applied to other blends (e.g., graphite–silicon anode).
Lithium-ion batteries play a vital role in a society more and more affected by the spectre of climate change: hence the need of lowering CO2 emissions and reducing the fossil fuel consumption. At the moment, lithium-ion batteries appear as the ideal candidates for this challenge but further research and development is required to understand their behaviour, predict their issues and therefore improve their performance. In this regard, mathematical modelling and numerical simulation have become standard techniques in lithium-ion battery research and development and have proven to be highly useful in supporting experimental work and increasing the predictability of model-based life expectancy.
This study focuses on the electrochemical ageing reactions at the anode, especially on the topic of lithium plating and its interaction with the solid electrolyte interface (SEI). The purpose of this work is a deeper understanding of these degradation processes through the construction of refined modelling frameworks and the analysis of simulations carried out over a wide range of operating conditions. The governing equations are implemented in the in-house multiphysics software package DENIS, while the electrochemistry model is based on the use of the open-source chemical kinetics code CANTERA.
The development, parameterisation and experimental validation of a comprehensive pseudo-three-dimensional multiphysics model of a commercial lithium-ion cell with blend cathode and graphite anode is presented. This model is able to describe and simulate both multiscale heat and mass transport and complex electrochemical reaction mechanisms, including also as extra feature the capability of reproducing a composite electrode where multiple active materials are subject to intercalation/deintercalation reaction.
A further extension to include reversible lithium plating process and predict ageing behaviour over a wide range of conditions, with a focus on the high currents and low temperatures particularly interesting for the fast charging topic, follows. This extended model is verified by comparison with published experimental data showing voltage plateau and voltage drop as plating indicators and optionally includes an explicit re-intercalation reaction that is shown to suppress macroscopic plating hints in the specific case of a cell not showing evident plating signs. This model is used to create degradation maps over a wide range of conditions and an in-depth spatiotemporal analysis of the anode behaviour at the mesoscopic and microscopic scales, demonstrating the dynamic and nonlinear interaction between the intercalation and plating reactions.
A deeper outlook on the SEI formation and growth is presented, together with the qualitative description of three different 1D-models with a decreasing level of detail, developed with the purpose of ideally being included in future in more comprehensive multiscale frameworks.
Finally, the extended model is successfully coupled with a previously developed SEI model to result in an original modelling framework able to simulate both degradation processes and their continuous positive feedback.
This article presents the development, parameterization, and experimental validation of a pseudo-three-dimensional (P3D) multiphysics model of a 350 mAh high-power lithium-ion pouch cell with graphite anode and lithium cobalt oxide/lithium nickel cobalt aluminum oxide (LCO/NCA) blend cathode. The model describes transport processes on three different scales: Heat transport on the macroscopic scale (cell), mass and charge transport on the mesoscopic scale (electrode pair), and mass transport on the microscopic scale (active material particles). A generalized description of electrochemistry in blend electrodes is developed, using the open-source software Cantera for calculating species source terms. Very good agreement of model predictions with galvanostatic charge/discharge measurements, electrochemical impedance spectroscopy, and surface temperature measurements is observed over a wide range of operating conditions (0.05C to 10C charge and discharge, 5°C to 35°C). The behavior of internal states (concentrations, potentials, temperatures) is discussed. The blend materials show a complex behavior with both intra-particle and inter-particle non-equilibria during cycling.
Fast charging of lithium-ion batteries remains one of the most delicate challenges for the automotive industry, being seriously affected by the formation of lithium metal in the negative electrode. Here we present a physicochemical pseudo-3D model that explicitly includes the plating reaction as side reaction running in parallel to the main intercalation reaction. The thermodynamics of the plating reaction are modeled depending on temperature and ion concentration, which differs from the often-used assumption of a constant plating condition of 0 V anode potential. The reaction kinetics are described with an Arrhenius-type rate law parameterized from an extensive literature research. Re-intercalation of plated lithium was modeled to take place either via reverse plating (solution-mediated) or via an explicit interfacial reaction (surface-mediated). At low temperatures not only the main processes (intercalation and solid-state diffusion) become slow, but also the plating reaction itself becomes slower. Using this model, we are able to predict typical macroscopic experimental observables that are indicative of plating, that is, a voltage plateau during discharge and a voltage drop upon temperature increase. A spatiotemporal analysis of the internal cell states allows a quantitative insight into the competition between intercalation and plating. Finally, we calculate operation maps over a wide range of C-rates and temperatures that allow to assess plating propensity as function of operating condition.